What Does Draw Ratio Mean for Deep-Draw Tray Lamination?

Film thins locally as it stretches over the tray surface; the higher the draw ratio, the worse the thinning. Deep-draw lamination requires draw-ratio control and pre-compensated thickness.

Draw ratio diagram (placeholder)

Draw-Ratio Essentials

Clear definition

Draw ratio = formed area / flat area, determining thinning.

Predictable thinning

Local thinning roughly tracks the draw ratio — compensate proportionally.

Rupture risk

Beyond the film's elongation limit, rupture occurs.

Tooling synergy

Corner radii and draft angles lower the effective draw ratio.

Draw-Ratio Control Reference

Measure per tray geometry.

Shallow trays< 1.5, standard lamination
Mid-depth1.5–2.5, compensation needed
Deep-draw> 2.5, thicker film + process optimization
PE elongation limit300%+
PLA elongation limit~30–100%
Design guidanceRadii ≥ 5 mm, draft ≥ 5°

Draw-Ratio FAQ

Where do deep-draw laminations fail?

Over-thinned corners and rupture, then wrinkles — fix with thickness compensation and larger radii.

Can we predict where it will break?

Yes — forming simulation predicts thinning distribution to guide film design.

Is PLA suitable for deep draws?

Its elongation is limited; prefer PP/PE or a lower-draw design.